{"id":363,"date":"2025-02-19T14:07:34","date_gmt":"2025-02-19T06:07:34","guid":{"rendered":"https:\/\/www.ampouletest.com\/?page_id=363"},"modified":"2026-02-02T08:15:20","modified_gmt":"2026-02-02T00:15:20","slug":"glass-grain-hydrolytic-resistance-tester-usp-iso","status":"publish","type":"page","link":"https:\/\/www.ampouletest.com\/fr\/glass-grain-hydrolytic-resistance-tester-usp-iso","title":{"rendered":"Test de r\u00e9sistance \u00e0 l'hydrolyse des grains de verre - USP\/ISO"},"content":{"rendered":"<div data-elementor-type=\"wp-page\" data-elementor-id=\"363\" class=\"elementor elementor-363\" data-elementor-post-type=\"page\">\n\t\t\t\t<div class=\"elementor-element elementor-element-c60fdbb e-flex e-con-boxed e-con e-parent\" data-id=\"c60fdbb\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-db6fcba e-con-full e-flex e-con e-child\" data-id=\"db6fcba\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-9d1f798 e-con-full e-flex e-con e-child\" data-id=\"9d1f798\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-8cc5a79 e-con-full e-flex e-con e-child\" data-id=\"8cc5a79\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-b6b67d4 elementor-widget elementor-widget-heading\" data-id=\"b6b67d4\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h1 class=\"elementor-heading-title elementor-size-default\">Testeur de r\u00e9sistance \u00e0 l'hydrolyse des grains de verre<\/h1>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-5a032b0 elementor-widget elementor-widget-heading\" data-id=\"5a032b0\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">ISO 719, ISO 720, USP 660<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-c754e2a elementor-widget elementor-widget-text-editor\" data-id=\"c754e2a\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Le testeur de r\u00e9sistance hydrolytique du grain de verre est un instrument essentiel pour \u00e9valuer la durabilit\u00e9 chimique des mat\u00e9riaux en verre, en particulier dans les emballages pharmaceutiques. Ce test \u00e9value la r\u00e9sistance du verre \u00e0 l'eau, un facteur important pour d\u00e9terminer comment un mat\u00e9riau interagira avec le contenu des r\u00e9cipients pharmaceutiques, tels que les bouteilles de perfusion et les flacons d'injection. En comprenant les principes et les normes qui sous-tendent ce test, les fabricants peuvent s'assurer que leurs emballages r\u00e9pondent aux exigences rigoureuses de l'industrie pharmaceutique.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-ef15f9e elementor-button-align-stretch elementor-widget elementor-widget-form\" data-id=\"ef15f9e\" data-element_type=\"widget\" data-settings=\"{&quot;button_width&quot;:&quot;20&quot;,&quot;step_next_label&quot;:&quot;Next&quot;,&quot;step_previous_label&quot;:&quot;Previous&quot;,&quot;step_type&quot;:&quot;number_text&quot;,&quot;step_icon_shape&quot;:&quot;circle&quot;}\" data-widget_type=\"form.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<form class=\"elementor-form\" method=\"post\" name=\"New Form\" action=\"\">\n\t\t\t<input type=\"hidden\" name=\"post_id\" value=\"363\"\/>\n\t\t\t<input type=\"hidden\" name=\"form_id\" value=\"ef15f9e\"\/>\n\t\t\t<input type=\"hidden\" name=\"referer_title\" value=\"Ampoule Test\" \/>\n\n\t\t\t\n\t\t\t<div class=\"elementor-form-fields-wrapper elementor-labels-above\">\n\t\t\t\t\t\t\t\t<div class=\"elementor-field-type-text elementor-field-group elementor-column elementor-field-group-name elementor-col-100 elementor-field-required\">\n\t\t\t\t\t\t\t\t\t\t\t\t<label for=\"form-field-name\" class=\"elementor-field-label\">\n\t\t\t\t\t\t\t\tNom\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t<input size=\"1\" type=\"text\" name=\"form_fields[name]\" id=\"form-field-name\" class=\"elementor-field elementor-size-sm  elementor-field-textual\" placeholder=\"Nom\" required=\"required\" aria-required=\"true\">\n\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<div class=\"elementor-field-type-text elementor-field-group elementor-column elementor-field-group-field_5634bb6 elementor-col-100\">\n\t\t\t\t\t\t\t\t\t\t\t\t<label for=\"form-field-field_5634bb6\" class=\"elementor-field-label\">\n\t\t\t\t\t\t\t\tEntreprise\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t<input size=\"1\" type=\"text\" name=\"form_fields[field_5634bb6]\" id=\"form-field-field_5634bb6\" class=\"elementor-field elementor-size-sm  elementor-field-textual\" placeholder=\"Entreprise\">\n\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<div class=\"elementor-field-type-email elementor-field-group elementor-column elementor-field-group-email elementor-col-100 elementor-field-required\">\n\t\t\t\t\t\t\t\t\t\t\t\t<label for=\"form-field-email\" class=\"elementor-field-label\">\n\t\t\t\t\t\t\t\tCourriel\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t<input size=\"1\" type=\"email\" name=\"form_fields[email]\" id=\"form-field-email\" class=\"elementor-field elementor-size-sm  elementor-field-textual\" placeholder=\"Courriel\" required=\"required\" aria-required=\"true\">\n\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<div class=\"elementor-field-type-textarea elementor-field-group elementor-column elementor-field-group-message elementor-col-100\">\n\t\t\t\t\t\t\t\t\t\t\t\t<label for=\"form-field-message\" class=\"elementor-field-label\">\n\t\t\t\t\t\t\t\tMessage\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t<textarea class=\"elementor-field-textual elementor-field  elementor-size-sm\" name=\"form_fields[message]\" id=\"form-field-message\" rows=\"4\" placeholder=\"Message\"><\/textarea>\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<div class=\"elementor-field-type-recaptcha_v3 elementor-field-group elementor-column elementor-field-group-field_d37acda elementor-col-100 recaptcha_v3-bottomright\">\n\t\t\t\t\t<div class=\"elementor-field\" id=\"form-field-field_d37acda\"><div class=\"elementor-g-recaptcha\" data-sitekey=\"6LeuX60rAAAAAElodUi54YrM7mqC6fGZX8tx93-Z\" data-type=\"v3\" data-action=\"Form\" data-badge=\"bottomright\" data-size=\"invisible\"><\/div><\/div>\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<div class=\"elementor-field-group elementor-column elementor-field-type-submit elementor-col-20 e-form__buttons\">\n\t\t\t\t\t<button class=\"elementor-button elementor-size-sm\" type=\"submit\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">Envoyer<\/span>\n\t\t\t\t\t\t\t\t\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/button>\n\t\t\t\t<\/div>\n\t\t\t<\/div>\n\t\t<input type=\"hidden\" name=\"trp-form-language\" value=\"fr\"\/><\/form>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-163fe1b e-con-full e-flex e-con e-child\" data-id=\"163fe1b\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-f29ff9c e-flex e-con-boxed e-con e-parent\" data-id=\"f29ff9c\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-fadf197 elementor-widget elementor-widget-heading\" data-id=\"fadf197\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Le r\u00f4le du testeur de r\u00e9sistance hydrolytique du grain de verre dans l'emballage pharmaceutique<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-7e073a9 elementor-widget elementor-widget-text-editor\" data-id=\"7e073a9\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>La fonction premi\u00e8re du test de r\u00e9sistance hydrolytique du grain de verre est d'\u00e9valuer comment les mat\u00e9riaux en verre r\u00e9agissent lorsqu'ils sont expos\u00e9s \u00e0 l'eau. Ce test est crucial pour les emballages en verre utilis\u00e9s dans l'industrie pharmaceutique, car un verre qui n'est pas suffisamment r\u00e9sistant \u00e0 l'eau pourrait laisser s'\u00e9chapper des produits chimiques qui affectent la stabilit\u00e9 des m\u00e9dicaments. Cela compromettrait en fin de compte la s\u00e9curit\u00e9 et l'efficacit\u00e9 des produits pharmaceutiques.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-fcfe601 e-flex e-con-boxed e-con e-parent\" data-id=\"fcfe601\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-285ac2f elementor-widget elementor-widget-heading\" data-id=\"285ac2f\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">M\u00e9thodologie d'essai : Comprendre les normes ISO 719 et ISO 720<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-030866f e-grid e-con-full e-con e-child\" data-id=\"030866f\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-a8ac35c e-con-full e-flex e-con e-child\" data-id=\"a8ac35c\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-b451adc elementor-widget elementor-widget-text-editor\" data-id=\"b451adc\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>La m\u00e9thode d'essai est d\u00e9crite dans les principales normes industrielles, \u00e0 savoir <a href=\"https:\/\/www.ampouletest.com\/fr\/iso-719-ampoule-glass-grains-test\/\"><strong data-start=\"1554\" data-end=\"1565\">ISO 719<\/strong><\/a> et <strong data-start=\"1570\" data-end=\"1581\">ISO 720<\/strong>. Ces normes fournissent des lignes directrices pr\u00e9cises sur la mani\u00e8re de r\u00e9aliser des essais de r\u00e9sistance hydrolytique sur le verre. En termes simples, l'\u00e9chantillon de verre est broy\u00e9 et expos\u00e9 \u00e0 de l'eau \u00e0 des temp\u00e9ratures \u00e9lev\u00e9es (98\u00b0C pour ISO 719, 121\u00b0C pour ISO 720). L'ampleur de l'attaque hydrolytique est d\u00e9termin\u00e9e en analysant l'alcali lib\u00e9r\u00e9 dans l'eau au cours du processus. Cette m\u00e9thode permet de classer le verre en fonction de sa r\u00e9sistance, ce qui garantit que le mat\u00e9riau r\u00e9pond aux normes de durabilit\u00e9 chimique requises pour les emballages pharmaceutiques.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-84508c7 e-con-full e-flex e-con e-child\" data-id=\"84508c7\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-ae4e97c elementor-widget elementor-widget-image\" data-id=\"ae4e97c\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<a href=\"https:\/\/www.ampouletest.com\/fr\/iso-719-ampoule-glass-grains-test\/\">\n\t\t\t\t\t\t\t<img fetchpriority=\"high\" decoding=\"async\" width=\"600\" height=\"200\" src=\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp\" class=\"attachment-large size-large wp-image-366\" alt=\"ISO 719\" srcset=\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp 600w, https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719-300x100.webp 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\t\t\t\t\t\t\t\t<\/a>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-3824347 elementor-widget elementor-widget-image\" data-id=\"3824347\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" width=\"600\" height=\"200\" src=\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-720.webp\" class=\"attachment-large size-large wp-image-365\" alt=\"ISO 720\" srcset=\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-720.webp 600w, https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-720-300x100.webp 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-6d5e9de e-flex e-con-boxed e-con e-parent\" data-id=\"6d5e9de\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-8e82f12 elementor-widget elementor-widget-heading\" data-id=\"8e82f12\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Caract\u00e9ristiques principales du testeur de r\u00e9sistance hydrolytique des grains de verre<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-b46b09e elementor-widget elementor-widget-text-editor\" data-id=\"b46b09e\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<ol data-start=\"2157\" data-end=\"3431\"><li data-start=\"2157\" data-end=\"2527\"><p data-start=\"2160\" data-end=\"2527\"><strong data-start=\"2160\" data-end=\"2192\">Pr\u00e9paration automatis\u00e9e des \u00e9chantillons<\/strong><br data-start=\"2192\" data-end=\"2195\" \/>Le mod\u00e8le GHR-01A du testeur automatise l'ensemble du processus de pr\u00e9paration des \u00e9chantillons. Les \u00e9chantillons de verre sont broy\u00e9s dans le mortier et un tamis vibrant s\u00e9pare les granul\u00e9s appropri\u00e9s, ce qui permet de rationaliser les tests et d'am\u00e9liorer la coh\u00e9rence des r\u00e9sultats. Ce processus automatis\u00e9 minimise l'erreur humaine et am\u00e9liore la pr\u00e9cision des tests.<\/p><\/li><li data-start=\"2529\" data-end=\"2836\"><p data-start=\"2532\" data-end=\"2836\"><strong data-start=\"2532\" data-end=\"2562\">Tests conformes aux normes<\/strong><br data-start=\"2562\" data-end=\"2565\" \/>Ce testeur est strictement conforme aux normes ISO, notamment ISO 719 et ISO 720, ce qui garantit que tous les tests sont conformes aux normes industrielles mondiales en mati\u00e8re de r\u00e9sistance \u00e0 l'hydrolyse. Le syst\u00e8me permet \u00e9galement de classer les mat\u00e9riaux en verre, ce qui est essentiel pour la conformit\u00e9 r\u00e9glementaire.<\/p><\/li><li data-start=\"2838\" data-end=\"3158\"><p data-start=\"2841\" data-end=\"3158\"><strong data-start=\"2841\" data-end=\"2874\">Pr\u00e9cision et s\u00e9curit\u00e9 accrues<\/strong><br data-start=\"2874\" data-end=\"2877\" \/>La conception de la machine int\u00e8gre diverses caract\u00e9ristiques de s\u00e9curit\u00e9, notamment la collecte automatis\u00e9e des d\u00e9chets de verre et le tamisage par vibration qui am\u00e9liore la pr\u00e9cision des r\u00e9sultats. Son syst\u00e8me intelligent minimise l'interaction humaine, r\u00e9duisant ainsi le risque de contamination ou d'endommagement des \u00e9chantillons.<\/p><\/li><li data-start=\"3160\" data-end=\"3431\"><p data-start=\"3163\" data-end=\"3431\"><strong data-start=\"3163\" data-end=\"3195\">Polyvalence et adaptabilit\u00e9<\/strong><br data-start=\"3195\" data-end=\"3198\" \/>Le testeur GHR-01A peut traiter une large gamme de mat\u00e9riaux en verre, y compris ceux utilis\u00e9s dans l'industrie pharmaceutique. Il s'adapte \u00e0 diff\u00e9rents types de verre, tels que ceux utilis\u00e9s dans les flacons m\u00e9dicaux, les ampoules et autres r\u00e9cipients.<\/p><\/li><\/ol>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-bbe91e5 e-flex e-con-boxed e-con e-parent\" data-id=\"bbe91e5\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-6c739f4 elementor-widget elementor-widget-heading\" data-id=\"6c739f4\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Importance des essais de r\u00e9sistance hydrolytique des grains de verre dans l'emballage<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-183e820 elementor-widget elementor-widget-text-editor\" data-id=\"183e820\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p data-start=\"3512\" data-end=\"3890\">Le test de r\u00e9sistance hydrolytique du grain de verre joue un r\u00f4le essentiel pour garantir la s\u00e9curit\u00e9 et la stabilit\u00e9 des produits pharmaceutiques. En adh\u00e9rant aux normes ISO 719 et ISO 720, les fabricants peuvent \u00e9valuer avec pr\u00e9cision si leurs emballages en verre r\u00e9sisteront \u00e0 l'exposition \u00e0 diverses substances, y compris l'eau. Cela permet d'\u00e9viter la contamination des m\u00e9dicaments et de garantir la s\u00e9curit\u00e9 des patients.<\/p><p data-start=\"3892\" data-end=\"4229\">En outre, ce processus d'essai contribue \u00e0 la long\u00e9vit\u00e9 et \u00e0 la fiabilit\u00e9 de l'emballage en verre. Les produits pharmaceutiques stock\u00e9s dans du verre \u00e0 faible r\u00e9sistance peuvent se d\u00e9t\u00e9riorer au fil du temps, ce qui compromet l'int\u00e9grit\u00e9 du produit. Le testeur de r\u00e9sistance hydrolytique permet de s'assurer que seuls des mat\u00e9riaux en verre de haute qualit\u00e9 sont utilis\u00e9s, minimisant ainsi le risque de d\u00e9gradation.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-3abc6b6 e-flex e-con-boxed e-con e-parent\" data-id=\"3abc6b6\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-5363c6b elementor-widget elementor-widget-heading\" data-id=\"5363c6b\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Applications dans diverses industries<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-bcd529d elementor-widget elementor-widget-text-editor\" data-id=\"bcd529d\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p data-start=\"4276\" data-end=\"4603\">Bien que le testeur de r\u00e9sistance hydrolytique du grain de verre soit principalement utilis\u00e9 dans l'industrie pharmaceutique, ses applications vont bien au-del\u00e0. Le testeur est \u00e9galement utilis\u00e9 dans la production d'autres produits en verre, tels que les r\u00e9cipients pour aliments, cosm\u00e9tiques et boissons, o\u00f9 la stabilit\u00e9 chimique du mat\u00e9riau est essentielle.<\/p><p data-start=\"4605\" data-end=\"4897\">Par exemple, les r\u00e9cipients en verre utilis\u00e9s pour les aliments et les boissons doivent r\u00e9sister aux attaques hydrolytiques pour garantir que leur contenu reste frais et propre \u00e0 la consommation. Dans ce cas, le testeur de r\u00e9sistance hydrolytique du grain de verre fournit des informations pr\u00e9cieuses sur l'ad\u00e9quation du mat\u00e9riau \u00e0 l'emballage.<\/p><p data-start=\"4920\" data-end=\"5448\">Le testeur de r\u00e9sistance hydrolytique du grain de verre est un outil essentiel pour garantir la durabilit\u00e9 chimique des mat\u00e9riaux en verre, en particulier dans l'industrie pharmaceutique. Gr\u00e2ce \u00e0 son adh\u00e9sion \u00e0 des normes internationales telles que ISO 719 et ISO 720, cet instrument aide les fabricants \u00e0 confirmer que leurs emballages ne compromettront pas la stabilit\u00e9 des m\u00e9dicaments qu'ils contiennent. En automatisant le processus de pr\u00e9paration des \u00e9chantillons et en garantissant des r\u00e9sultats pr\u00e9cis et normalis\u00e9s, le testeur est indispensable au contr\u00f4le de la qualit\u00e9 dans diverses industries.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-afc7507 e-flex e-con-boxed e-con e-parent\" data-id=\"afc7507\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-6172ff6 elementor-widget elementor-widget-heading\" data-id=\"6172ff6\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Foire aux questions (FAQ)<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-dc8ba56 elementor-widget elementor-widget-n-accordion\" data-id=\"dc8ba56\" data-element_type=\"widget\" data-settings=\"{&quot;default_state&quot;:&quot;expanded&quot;,&quot;max_items_expended&quot;:&quot;one&quot;,&quot;n_accordion_animation_duration&quot;:{&quot;unit&quot;:&quot;ms&quot;,&quot;size&quot;:400,&quot;sizes&quot;:[]}}\" data-widget_type=\"nested-accordion.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"e-n-accordion\" aria-label=\"Accord\u00e9on. Ouvrez les liens avec Enter ou Space, fermez-les avec Escape et naviguez avec les touches fl\u00e9ch\u00e9es.\">\n\t\t\t\t\t\t<details id=\"e-n-accordion-item-2310\" class=\"e-n-accordion-item\" open>\n\t\t\t\t<summary class=\"e-n-accordion-item-title\" data-accordion-index=\"1\" tabindex=\"0\" aria-expanded=\"true\" aria-controls=\"e-n-accordion-item-2310\" >\n\t\t\t\t\t<span class='e-n-accordion-item-title-header'><div class=\"e-n-accordion-item-title-text\"> 1. \u00c0 quoi sert le testeur de r\u00e9sistance hydrolytique des grains de verre ? <\/div><\/span>\n\t\t\t\t\t\t\t<span class='e-n-accordion-item-title-icon'>\n\t\t\t<span class='e-opened' ><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-minus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h384c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t\t<span class='e-closed'><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-plus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H272V64c0-17.67-14.33-32-32-32h-32c-17.67 0-32 14.33-32 32v144H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h144v144c0 17.67 14.33 32 32 32h32c17.67 0 32-14.33 32-32V304h144c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t<\/span>\n\n\t\t\t\t\t\t<\/summary>\n\t\t\t\t<div role=\"region\" aria-labelledby=\"e-n-accordion-item-2310\" class=\"elementor-element elementor-element-6687fad e-con-full e-flex e-con e-child\" data-id=\"6687fad\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-7661576 elementor-widget elementor-widget-text-editor\" data-id=\"7661576\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Le testeur de r\u00e9sistance hydrolytique du grain de verre est utilis\u00e9 pour \u00e9valuer la durabilit\u00e9 chimique des mat\u00e9riaux en verre, en particulier dans les emballages pharmaceutiques, afin de s'assurer qu'ils ne lib\u00e8rent pas de substances nocives dans le contenu.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/details>\n\t\t\t\t\t\t<details id=\"e-n-accordion-item-2311\" class=\"e-n-accordion-item\" >\n\t\t\t\t<summary class=\"e-n-accordion-item-title\" data-accordion-index=\"2\" tabindex=\"-1\" aria-expanded=\"false\" aria-controls=\"e-n-accordion-item-2311\" >\n\t\t\t\t\t<span class='e-n-accordion-item-title-header'><div class=\"e-n-accordion-item-title-text\"> 2. Quelles sont les normes \u00e0 respecter pour le test de r\u00e9sistance \u00e0 l'hydrolyse ? <\/div><\/span>\n\t\t\t\t\t\t\t<span class='e-n-accordion-item-title-icon'>\n\t\t\t<span class='e-opened' ><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-minus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h384c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t\t<span class='e-closed'><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-plus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H272V64c0-17.67-14.33-32-32-32h-32c-17.67 0-32 14.33-32 32v144H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h144v144c0 17.67 14.33 32 32 32h32c17.67 0 32-14.33 32-32V304h144c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t<\/span>\n\n\t\t\t\t\t\t<\/summary>\n\t\t\t\t<div role=\"region\" aria-labelledby=\"e-n-accordion-item-2311\" class=\"elementor-element elementor-element-f898b88 e-con-full e-flex e-con e-child\" data-id=\"f898b88\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-7acc6e6 elementor-widget elementor-widget-text-editor\" data-id=\"7acc6e6\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p><span style=\"font-size: 16px;\">Le test est conforme \u00e0 <\/span><strong style=\"font-size: 16px;\" data-start=\"5882\" data-end=\"5893\">ISO 719<\/strong><span style=\"font-size: 16px;\"> et <\/span><strong style=\"font-size: 16px;\" data-start=\"5898\" data-end=\"5909\">ISO 720<\/strong><span style=\"font-size: 16px;\">qui fournissent des lignes directrices pour l'\u00e9valuation de la r\u00e9sistance du verre aux attaques hydrolytiques \u00e0 diff\u00e9rentes temp\u00e9ratures.<\/span><\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/details>\n\t\t\t\t\t\t<details id=\"e-n-accordion-item-2312\" class=\"e-n-accordion-item\" >\n\t\t\t\t<summary class=\"e-n-accordion-item-title\" data-accordion-index=\"3\" tabindex=\"-1\" aria-expanded=\"false\" aria-controls=\"e-n-accordion-item-2312\" >\n\t\t\t\t\t<span class='e-n-accordion-item-title-header'><div class=\"e-n-accordion-item-title-text\"> 3. Quelles sont les principales caract\u00e9ristiques du testeur de r\u00e9sistance \u00e0 l'hydrolyse des grains de verre GHR-01A ? <\/div><\/span>\n\t\t\t\t\t\t\t<span class='e-n-accordion-item-title-icon'>\n\t\t\t<span class='e-opened' ><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-minus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h384c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t\t<span class='e-closed'><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-plus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H272V64c0-17.67-14.33-32-32-32h-32c-17.67 0-32 14.33-32 32v144H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h144v144c0 17.67 14.33 32 32 32h32c17.67 0 32-14.33 32-32V304h144c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t<\/span>\n\n\t\t\t\t\t\t<\/summary>\n\t\t\t\t<div role=\"region\" aria-labelledby=\"e-n-accordion-item-2312\" class=\"elementor-element elementor-element-16b3991 e-con-full e-flex e-con e-child\" data-id=\"16b3991\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-0f22f6a elementor-widget elementor-widget-text-editor\" data-id=\"0f22f6a\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Le GHR-01A se caract\u00e9rise par une pr\u00e9paration automatis\u00e9e des \u00e9chantillons, un tamisage vibrant, des mesures de s\u00e9curit\u00e9 et une conformit\u00e9 aux normes internationales, ce qui permet d'am\u00e9liorer la pr\u00e9cision et l'efficacit\u00e9 des tests.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/details>\n\t\t\t\t\t\t<details id=\"e-n-accordion-item-2313\" class=\"e-n-accordion-item\" >\n\t\t\t\t<summary class=\"e-n-accordion-item-title\" data-accordion-index=\"4\" tabindex=\"-1\" aria-expanded=\"false\" aria-controls=\"e-n-accordion-item-2313\" >\n\t\t\t\t\t<span class='e-n-accordion-item-title-header'><div class=\"e-n-accordion-item-title-text\"> 4. Comment fonctionne le processus de test ? <\/div><\/span>\n\t\t\t\t\t\t\t<span class='e-n-accordion-item-title-icon'>\n\t\t\t<span class='e-opened' ><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-minus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h384c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t\t<span class='e-closed'><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-plus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H272V64c0-17.67-14.33-32-32-32h-32c-17.67 0-32 14.33-32 32v144H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h144v144c0 17.67 14.33 32 32 32h32c17.67 0 32-14.33 32-32V304h144c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t<\/span>\n\n\t\t\t\t\t\t<\/summary>\n\t\t\t\t<div role=\"region\" aria-labelledby=\"e-n-accordion-item-2313\" class=\"elementor-element elementor-element-e72fc80 e-flex e-con-boxed e-con e-child\" data-id=\"e72fc80\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-4987009 elementor-widget elementor-widget-text-editor\" data-id=\"4987009\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Les grains de verre sont broy\u00e9s, plac\u00e9s dans un bain chauffant et expos\u00e9s \u00e0 de l'eau \u00e0 haute temp\u00e9rature. L'alcali lib\u00e9r\u00e9 par le verre est mesur\u00e9 pour \u00e9valuer sa r\u00e9sistance \u00e0 l'hydrolyse.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/details>\n\t\t\t\t\t\t<details id=\"e-n-accordion-item-2314\" class=\"e-n-accordion-item\" >\n\t\t\t\t<summary class=\"e-n-accordion-item-title\" data-accordion-index=\"5\" tabindex=\"-1\" aria-expanded=\"false\" aria-controls=\"e-n-accordion-item-2314\" >\n\t\t\t\t\t<span class='e-n-accordion-item-title-header'><div class=\"e-n-accordion-item-title-text\"> 5. Ce testeur peut-il \u00eatre utilis\u00e9 pour d'autres types de verre ? <\/div><\/span>\n\t\t\t\t\t\t\t<span class='e-n-accordion-item-title-icon'>\n\t\t\t<span class='e-opened' ><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-minus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h384c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t\t<span class='e-closed'><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-plus\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M416 208H272V64c0-17.67-14.33-32-32-32h-32c-17.67 0-32 14.33-32 32v144H32c-17.67 0-32 14.33-32 32v32c0 17.67 14.33 32 32 32h144v144c0 17.67 14.33 32 32 32h32c17.67 0 32-14.33 32-32V304h144c17.67 0 32-14.33 32-32v-32c0-17.67-14.33-32-32-32z\"><\/path><\/svg><\/span>\n\t\t<\/span>\n\n\t\t\t\t\t\t<\/summary>\n\t\t\t\t<div role=\"region\" aria-labelledby=\"e-n-accordion-item-2314\" class=\"elementor-element elementor-element-d46eb70 e-flex e-con-boxed e-con e-child\" data-id=\"d46eb70\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-ceaf7bc elementor-widget elementor-widget-text-editor\" data-id=\"ceaf7bc\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Oui, le testeur peut \u00eatre utilis\u00e9 pour diff\u00e9rents types de mat\u00e9riaux en verre, y compris ceux utilis\u00e9s dans les emballages pharmaceutiques, alimentaires et cosm\u00e9tiques, pour autant qu'ils r\u00e9pondent aux sp\u00e9cifications requises.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/details>\n\t\t\t\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>","protected":false},"excerpt":{"rendered":"<p>Testeur de r\u00e9sistance hydrolytique du grain de verre ISO 719, ISO 720, USP 660 Le testeur de r\u00e9sistance hydrolytique du grain de verre est un instrument essentiel pour \u00e9valuer la durabilit\u00e9 chimique des mat\u00e9riaux en verre, en particulier dans les emballages pharmaceutiques. Ce test \u00e9value la r\u00e9sistance du verre \u00e0 l'eau, un facteur important pour d\u00e9terminer comment un mat\u00e9riau interagira avec le contenu de [...]<\/p>","protected":false},"author":3,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"footnotes":""},"class_list":["post-363","page","type-page","status-publish","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO plugin v24.2 - https:\/\/yoast.com\/wordpress\/plugins\/seo\/ -->\n<title>Glass Grain Hydrolytic Resistance Tester - Ampoule Test<\/title>\n<meta name=\"description\" content=\"How the Glass Grain Hydrolytic Resistance Tester ensures the durability of glass material for ampoule. Learn about ISO 719, ISO 720, USP 660.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/www.ampouletest.com\/fr\/glass-grain-hydrolytic-resistance-tester-usp-iso\/\" \/>\n<meta property=\"og:locale\" content=\"fr_FR\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"Glass Grain Hydrolytic Resistance Tester - Ampoule Test\" \/>\n<meta property=\"og:description\" content=\"How the Glass Grain Hydrolytic Resistance Tester ensures the durability of glass material for ampoule. Learn about ISO 719, ISO 720, USP 660.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/www.ampouletest.com\/fr\/glass-grain-hydrolytic-resistance-tester-usp-iso\/\" \/>\n<meta property=\"og:site_name\" content=\"Ampoule Test\" \/>\n<meta property=\"article:modified_time\" content=\"2026-02-02T00:15:20+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp\" \/>\n\t<meta property=\"og:image:width\" content=\"600\" \/>\n\t<meta property=\"og:image:height\" content=\"200\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/webp\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Dur\u00e9e de lecture estim\u00e9e\" \/>\n\t<meta name=\"twitter:data1\" content=\"6 minutes\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\/\/schema.org\",\"@graph\":[{\"@type\":\"WebPage\",\"@id\":\"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso\",\"url\":\"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso\",\"name\":\"Glass Grain Hydrolytic Resistance Tester - Ampoule Test\",\"isPartOf\":{\"@id\":\"https:\/\/www.ampouletest.com\/#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#primaryimage\"},\"image\":{\"@id\":\"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#primaryimage\"},\"thumbnailUrl\":\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp\",\"datePublished\":\"2025-02-19T06:07:34+00:00\",\"dateModified\":\"2026-02-02T00:15:20+00:00\",\"description\":\"How the Glass Grain Hydrolytic Resistance Tester ensures the durability of glass material for ampoule. Learn about ISO 719, ISO 720, USP 660.\",\"breadcrumb\":{\"@id\":\"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#breadcrumb\"},\"inLanguage\":\"fr-FR\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"fr-FR\",\"@id\":\"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#primaryimage\",\"url\":\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp\",\"contentUrl\":\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp\"},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"Home\",\"item\":\"https:\/\/www.ampouletest.com\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Glass Grain Hydrolytic Resistance Tester \u2013 USP\/ISO\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\/\/www.ampouletest.com\/#website\",\"url\":\"https:\/\/www.ampouletest.com\/\",\"name\":\"Softgel Test\",\"description\":\"Ampoule Test Solutions\",\"publisher\":{\"@id\":\"https:\/\/www.ampouletest.com\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\/\/www.ampouletest.com\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"fr-FR\"},{\"@type\":\"Organization\",\"@id\":\"https:\/\/www.ampouletest.com\/#organization\",\"name\":\"Softgel Test\",\"url\":\"https:\/\/www.ampouletest.com\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"fr-FR\",\"@id\":\"https:\/\/www.ampouletest.com\/#\/schema\/logo\/image\/\",\"url\":\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/01\/Softgel-Test-Logo.webp\",\"contentUrl\":\"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/01\/Softgel-Test-Logo.webp\",\"width\":836,\"height\":238,\"caption\":\"Softgel Test\"},\"image\":{\"@id\":\"https:\/\/www.ampouletest.com\/#\/schema\/logo\/image\/\"}}]}<\/script>\n<!-- \/ Yoast SEO plugin. -->","yoast_head_json":{"title":"Glass Grain Hydrolytic Resistance Tester - Ampoule Test","description":"How the Glass Grain Hydrolytic Resistance Tester ensures the durability of glass material for ampoule. Learn about ISO 719, ISO 720, USP 660.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/www.ampouletest.com\/fr\/glass-grain-hydrolytic-resistance-tester-usp-iso\/","og_locale":"fr_FR","og_type":"article","og_title":"Glass Grain Hydrolytic Resistance Tester - Ampoule Test","og_description":"How the Glass Grain Hydrolytic Resistance Tester ensures the durability of glass material for ampoule. Learn about ISO 719, ISO 720, USP 660.","og_url":"https:\/\/www.ampouletest.com\/fr\/glass-grain-hydrolytic-resistance-tester-usp-iso\/","og_site_name":"Ampoule Test","article_modified_time":"2026-02-02T00:15:20+00:00","og_image":[{"width":600,"height":200,"url":"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp","type":"image\/webp"}],"twitter_card":"summary_large_image","twitter_misc":{"Dur\u00e9e de lecture estim\u00e9e":"6 minutes"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"WebPage","@id":"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso","url":"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso","name":"Glass Grain Hydrolytic Resistance Tester - Ampoule Test","isPartOf":{"@id":"https:\/\/www.ampouletest.com\/#website"},"primaryImageOfPage":{"@id":"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#primaryimage"},"image":{"@id":"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#primaryimage"},"thumbnailUrl":"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp","datePublished":"2025-02-19T06:07:34+00:00","dateModified":"2026-02-02T00:15:20+00:00","description":"How the Glass Grain Hydrolytic Resistance Tester ensures the durability of glass material for ampoule. Learn about ISO 719, ISO 720, USP 660.","breadcrumb":{"@id":"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#breadcrumb"},"inLanguage":"fr-FR","potentialAction":[{"@type":"ReadAction","target":["https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso"]}]},{"@type":"ImageObject","inLanguage":"fr-FR","@id":"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#primaryimage","url":"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp","contentUrl":"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/02\/ISO-719.webp"},{"@type":"BreadcrumbList","@id":"https:\/\/www.ampouletest.com\/glass-grain-hydrolytic-resistance-tester-usp-iso#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Home","item":"https:\/\/www.ampouletest.com\/"},{"@type":"ListItem","position":2,"name":"Glass Grain Hydrolytic Resistance Tester \u2013 USP\/ISO"}]},{"@type":"WebSite","@id":"https:\/\/www.ampouletest.com\/#website","url":"https:\/\/www.ampouletest.com\/","name":"Softgel Test","description":"Ampoule Test Solutions","publisher":{"@id":"https:\/\/www.ampouletest.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/www.ampouletest.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"fr-FR"},{"@type":"Organization","@id":"https:\/\/www.ampouletest.com\/#organization","name":"Softgel Test","url":"https:\/\/www.ampouletest.com\/","logo":{"@type":"ImageObject","inLanguage":"fr-FR","@id":"https:\/\/www.ampouletest.com\/#\/schema\/logo\/image\/","url":"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/01\/Softgel-Test-Logo.webp","contentUrl":"https:\/\/www.ampouletest.com\/wp-content\/uploads\/2025\/01\/Softgel-Test-Logo.webp","width":836,"height":238,"caption":"Softgel Test"},"image":{"@id":"https:\/\/www.ampouletest.com\/#\/schema\/logo\/image\/"}}]}},"_links":{"self":[{"href":"https:\/\/www.ampouletest.com\/fr\/wp-json\/wp\/v2\/pages\/363","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.ampouletest.com\/fr\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/www.ampouletest.com\/fr\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/www.ampouletest.com\/fr\/wp-json\/wp\/v2\/users\/3"}],"replies":[{"embeddable":true,"href":"https:\/\/www.ampouletest.com\/fr\/wp-json\/wp\/v2\/comments?post=363"}],"version-history":[{"count":5,"href":"https:\/\/www.ampouletest.com\/fr\/wp-json\/wp\/v2\/pages\/363\/revisions"}],"predecessor-version":[{"id":662,"href":"https:\/\/www.ampouletest.com\/fr\/wp-json\/wp\/v2\/pages\/363\/revisions\/662"}],"wp:attachment":[{"href":"https:\/\/www.ampouletest.com\/fr\/wp-json\/wp\/v2\/media?parent=363"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}